Random-pattern slabs: care and expectations

Pattern and colour variation are intentional, but damage and contamination are not. Here is how to care for the surface and set the right expectations.

How random pattern works

Random pattern applies to both Silestone and Dekton. A varied pattern gives a natural-stone look. No two slabs are identical.

Variation, pattern direction and joint placement look different across a whole slab than on a small sample. Customer photos make it easier to assess that larger scale.

Design, not a defect

Varying veins and tones are part of the colour. Lay the slab out before cutting so that the look can be approved. Show the customer the slab and explain the natural variation, including what is part of the design and what is grounds for a claim.

Match the flow

Mark the joints and turn the pieces until the vein flow lines up. Take photos to show the customer.

Tone number

Check the tone numbers on the tags and also compare the slabs visually in the same light. The tag does not guarantee that tones and patterns will match.

Care: the same routine, more forgiving

The pattern hides small marks but needs the same gentle cleaning.

Mild products

Washing-up liquid or a mild all-purpose cleaner on a soft cloth. Harsh chemicals can attack the pigments, so follow the standard care and maintenance advice.

Wipe dry

Water marks show less on a patterned surface but can leave dull patches over time. Wipe dry, especially on dark random-pattern colours.

When is it a claim?

The difference between design variation and a defect under slab quality control.

Contamination

For Dekton, contamination exceeding 1 mm in length or width or 0.7 mm in height is non-compliant. Dots smaller than 1 mm are also non-compliant if visible from 700 mm away at an angle of 45 degrees. For Dekton, geometrically defined inkjet strips longer than 200 mm, parallel to the long side of the slab, must also be assessed under the quality manual. Document them before cutting.

Edge chips and cracks

These must be marked and written off before fabrication. The customer must not receive visible defects.

Thickness and flatness

For Dekton, thickness must be within ±0.5 mm and flatness deviation below 2 mm on a calibrated flat surface. For Silestone, thickness must be within ±1 mm, with flatness deviation below 3 mm across the slab and below 5 mm along it. Deviations outside the tolerances for the relevant material must be rejected before delivery.

Frequently asked questions

Is a varying pattern a defect?

No. Random pattern means veins and tones that vary on purpose. Every slab is unique and should be laid out and matched before cutting.

Do marks show more or less?

The pattern can hide small marks, but strong stains still show. Clean them up quickly, using the same mild products as on other slabs.

How do I match several slabs?

Lay them out face to face, mark the joints and follow the vein flow. Check the tone numbers on the tags and compare the slabs visually in the same light.

What can be claimed?

Contamination, printing faults, cracks and dimensions outside tolerance must be assessed under the quality manual for Dekton or Silestone. The contamination and inkjet strip limits in this guide apply to Dekton. The variation in the pattern, however, is design.